Standard Guide for Use of Adhesive-Bonded Single Lap-Joint Specimen Test Results
Přeložit název
NORMA vydána dne 1.5.2016
Označení normy: ASTM D4896-01(2016)
Poznámka: NEPLATNÁ
Datum vydání normy: 1.5.2016
Kód zboží: NS-638452
Počet stran: 6
Přibližná hmotnost: 18 g (0.04 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
shear strength, single-lap joint, tension loading,, ICS Number Code 83.180 (Adhesives)
Significance and Use | ||||||||||||||||||||||||||||||||||||||||||||||||||
4.1 Single-lap specimens are economical, practical, and easy to make. They are the most widely used specimens for development, evaluation, and comparative studies involving adhesives and bonded products, including manufacturing quality control. 4.2 Special specimens and test methods have been developed that yield accurate estimates of the true shear strength of adhesives. These methods eliminate or minimize many of the deficiencies of the thin-adherend single-lap specimens, but are more difficult to make and test. (See Test Methods D3983, D4027, D4562, and E229.) 4.3 The misuse of strength values obtained from such Test Methods or Practices as D906, D1002, D1144, D1151, D1183, D1780, D2294, D2295, D2339, D3163, D3164, D3165, D3434, D3528, D3632, and D5868, as allowable design-stress values for structural joints could lead to product failure, property damage, and human injury. |
||||||||||||||||||||||||||||||||||||||||||||||||||
1. Scope | ||||||||||||||||||||||||||||||||||||||||||||||||||
1.1 This guide is directed toward the safe and appropriate use of strength values obtained from test methods using single-lap adhesive joint specimens. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 The discussion focuses on shear strength as measured with small thin-adherend, single-lap specimens. Many factors, however, apply to shear modulus, tensile strength, and tensile modulus measured by small laboratory specimens in general. This discussion is limited to single-lap specimens and shear strength only for simplification. |
||||||||||||||||||||||||||||||||||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||||||||||||||||||||||||||||||||||
|
Chcete pravidelně odebírat informace o nově vycházejících normách z celého světa a to zcela zdarma?
Přihlašte se k odběru. Vše je velice jednoduché a absolutně ZDARMA.
Na výběr máte vydavatele z celého světa.
Poslední aktualizace: 22.12.2024 (Počet položek: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.