Standard Specification for Nickel Rod and Bar (Includes all amendments And changes 10/8/2014).
Automaticky přeložený název:
Standardní specifikace pro Nickel tyč
NORMA vydána dne 1.10.2009
Označení normy: ASTM B160-05(2009)e1
Poznámka: NEPLATNÁ
Datum vydání normy: 1.10.2009
Kód zboží: NS-5521
Počet stran: 6
Přibližná hmotnost: 18 g (0.04 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
bar, rod, N02200, N02201, N02211, Nickel--specifications, Nickel alloy rod/bar/wire--specifications, UNS N02200 (commercially pure Ni alloy, Nickel 200), UNS N02201 (commercially pure Ni alloy, Nickel 201), ICS Number Code 2211, 77.150.40 (Nickel and chromium products)
1. Scope | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
1.1 This specification covers nickel (UNS N02200)*, low carbon nickel (UNS N02201)*, and solution strengthened nickel (UNS N02211) in the form of hot-worked and cold-worked rod and bar in the conditions shown in Table 1. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use. TABLE 1 Mechanical Properties
A See 12.2. B Not applicable to diameters or cross sections under 3/32 in. (2.4 mm). C For hot-worked flats 5/16 in. (7.9 mm) and under in thickness the elongation shall be 25%, min. D Hardness B45 to B80, or equivalent. E Hardness B45 to B70 or equivalent. F Forging quality is furnished to chemical requirements and surface inspection only. No tensile properties are required. |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
Chcete mít jistotu o platnosti užívaných předpisů?
Nabízíme Vám řešení, abyste mohli používat stále platné (aktuální) legislativní předpisy.
Chcete vědět více informací? Podívejte se na tuto stránku.
Poslední aktualizace: 15.05.2024 (Počet položek: 2 900 316)
© Copyright 2024 NORMSERVIS s.r.o.