Potřebujeme váš souhlas k využití jednotlivých dat, aby se vám mimo jiné mohly ukazovat informace týkající se vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.
Standard Test Methods for Tension Testing of Metallic Materials
Automaticky přeložený název:
Standardní zkušební metody pro Tension zkoušení kovových materiálů
NORMA vydána dne 1.4.2004
Označení normy: ASTM E8-04
Poznámka: NEPLATNÁ
Datum vydání normy: 1.4.2004
Kód zboží: NS-48035
Počet stran: 24
Přibližná hmotnost: 72 g (0.16 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
accuracy, bending stress, discontinuous yielding, drop-of-the-beam, eccentric force application, elastic extension, elongation, extension-under-load, extensometer, force, free-running crosshead speed, gage length, halt-of-the force, percent elongation, plastic extension, preload, rate of stressing, rate of straining, reduced section, reduction of area, sensitivity, strain, stress, taring, tensile strength, tension testing, yield point elongation, yield strength
Significance and Use |
Tension tests provide information on the strength and ductility of materials under uniaxial tensile stresses. This information may be useful in comparisons of materials, alloy development, quality control, and design under certain circumstances. The results of tension tests of specimens machined to standardized dimensions from selected portions of a part or material may not totally represent the strength and ductility properties of the entire end product or its in-service behavior in different environments. These test methods are considered satisfactory for acceptance testing of commercial shipments. The test methods have been used extensively in the trade for this purpose. |
1. Scope |
1.1 These test methods cover the tension testing of metallic materials in any form at room temperature, specifically, the methods of determination of yield strength, yield point elongation, tensile strength, elongation, and reduction of area. Note 1-A complete metric companion to Test Methods E 8 has been developed, therefore, no metric equivalents are shown in these test methods. Committee E28 was granted an exception in 1997 by the Committee on Standards to maintain E8 and E8M as separate companion standards rather than combining standards as recommended by the Form and Style Manual. Note 2-Gage lengths in these test methods are required to be 4D for most round specimens. Test specimens made from powder metallurgy (P/M) materials are exempt from this requirement by industry-wide agreement to keep the pressing of the material to a specific projected area and density. Note 3-Exceptions to the provisions of these test methods may need to be made in individual specifications or test methods for a particular material. For examples, see Test Methods and Definitions A 370 and Test Methods B 557. Note 4-Room temperature shall be considered to be 50 to 100F unless otherwise specified. 1.2This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
Chcete mít jistotu, že používáte pouze platné technické normy?
Nabízíme Vám řešení, které Vám zajistí měsíční přehled o aktuálnosti norem, které používáte.
Chcete vědět více informací? Podívejte se na tuto stránku.
Poslední aktualizace: 21.11.2024 (Počet položek: 2 206 478)
© Copyright 2024 NORMSERVIS s.r.o.