Standard Test Method for Determination of Moderately High Temperature Piston Deposits by Thermo-Oxidation Engine Oil Simulation Test-TEOST MHT
Automaticky přeložený název:
Standardní zkušební metoda pro stanovení středně vysoké teploty pístů Vklady od termooxidačních Motorový olej simulační test-TEOST MHT
NORMA vydána dne 1.6.2009
Označení normy: ASTM D7097-09
Poznámka: NEPLATNÁ
Datum vydání normy: 1.6.2009
Kód zboží: NS-37536
Počet stran: 14
Přibližná hmotnost: 42 g (0.09 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
deposits, engine oil, oxidation, thermal decomposition, thermal oxidation, Engine (lubricating) oils, Piston deposits, TEOST (thermo-oxidation engine oil simulation test), Thermal decomposition, Thermal oxidation, ICS Number Code 75.100 (Lubricants, industrial oils and related products)
Significance and Use | ||||
The test method is designed to predict the deposit-forming tendencies of engine oil in the piston ring belt and upper piston crown area. Correlation has been shown between the TEOST MHT procedure and the TU3MH Peugeot engine test in deposit formation. Such deposits formed in the ring-belt area of a reciprocating engine piston can cause problems with engine operation and longevity. It is one of the required test methods in Specification D 4485 to define API Category-Identified engine oils. |
||||
1. Scope | ||||
1.1 This test method covers the procedure to determine the mass of deposit formed on a specially constructed test rod exposed to repetitive passage of 8.5 g of engine oil over the rod in a thin film under oxidative and catalytic conditions at 285°C. The range of applicability of the Moderately High Temperature Thermo-Oxidation Engine Test (TEOST MHT ) test method as derived from an interlaboratory study is approximately 10 to 100 mg. However, experience indicates that deposit values from 1 to 150 mg or greater may be obtained. 1.2 This test method uses a patented instrument, method and patented, numbered, and registered depositor rods traceable to the manufacturer and made specifically for the practice and precision of the test method. 1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.3.1 The values stated in SI units are to be regarded as standard. Although not an SI unit, the special name, litre (L) is allowed by SI for the cubic decimetre (dm3) and the millilitre (mL) for the SI cubic centimetre (cm3). 1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||
2. Referenced Documents | ||||
|
Historická
15.2.2011
Historická
1.1.2011
Historická
15.6.2011
Historická
1.1.2011
Historická
1.5.2011
Historická
1.7.2011
Poslední aktualizace: 22.12.2024 (Počet položek: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.