Potřebujeme váš souhlas k využití jednotlivých dat, aby se vám mimo jiné mohly ukazovat informace týkající se vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.
Standard Test Method for Determining Tensile Properties of Nonreinforced Polyethylene and Nonreinforced Flexible Polypropylene Geomembranes
Automaticky přeložený název:
Standardní zkušební metoda pro stanovení mechanických vlastností Nonreinforced polyethylenu a Nonreinforced flexibilní polypropylenové geomembrán
NORMA vydána dne 1.6.2004
Označení normy: ASTM D6693-04
Poznámka: NEPLATNÁ
Datum vydání normy: 1.6.2004
Kód zboží: NS-36169
Počet stran: 5
Přibližná hmotnost: 15 g (0.03 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
nonreinforced, percent break elongation, percent yield elongation, polyethylene, polypropylene, tensile break strength, tensile yield strength, ICS Number Code 59.080.70 (Geotextiles)
1. Scope | ||||||||||||||
1.1 This test method covers the determination of the tensile properties of nonreinforced geomembranes in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature and machine speed. 1.2 This test method can be used for testing materials thickness between 0.25 mm (0.010 in) and 6.3 mm (0.25 in.). Note 1—This test method is not intended to cover precise physical procedures. The constant rate of crosshead movement of this test lacks accuracy from a theoretical standpoint. A wide difference may exist between the rate of crosshead movement and the rate of strain of the specimen indicating that the testing speeds specified may disguise important effects or characteristics of these materials in the plastic state. Further, it is realized that variations in the thicknesses of test specimen, as permitted by this test standard, produce variations in the surface-volume ratios of such specimens, and that these variations may influence the test results. Hence, where directly comparable results are desired, all samples should be of equal thickness. Special additional tests should be used where more precise physical data are needed. 1.3 Test data obtained by this test method is relevant and may be appropriate for use in engineering design with consideration of test conditions as compared to in-service conditions. 1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||
2. Referenced Documents | ||||||||||||||
|
Chcete mít jistotu, že používáte pouze platné technické normy?
Nabízíme Vám řešení, které Vám zajistí měsíční přehled o aktuálnosti norem, které používáte.
Chcete vědět více informací? Podívejte se na tuto stránku.
Poslední aktualizace: 22.11.2024 (Počet položek: 2 206 568)
© Copyright 2024 NORMSERVIS s.r.o.