Potřebujeme váš souhlas k využití jednotlivých dat, aby se vám mimo jiné mohly ukazovat informace týkající se vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.
Standard Test Method for Tensile Strength at Zero-Span (""Wet Zero-Span Tensile"")
Automaticky přeložený název:
Standardní zkušební metoda pro pevnost v tahu Zero - Span ( " Wet Zero- Span tahu " )
NORMA vydána dne 10.12.1997
Označení normy: ASTM D5803-97
Poznámka: NEPLATNÁ
Datum vydání normy: 10.12.1997
Kód zboží: NS-32626
Počet stran: 6
Přibližná hmotnost: 18 g (0.04 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
Paper, "Wet zero-span tensile" test, Zero span tests, wet tensile strength at zero-span, test,, Tension (tensile) properties/tests-paper products, wet tensile strengthat zero-span
1. Scope | ||||||||||||||
1.1 This test method provides a quick, reliable means to measure the wet zero-span tensile strength of a specimen of sheeted material. 1.2 In cases where fibers are to be tested prior to finished production of paper or paperboard, a random standard aggregate of pulp fibers, or handsheet, produced using a standardized procedure, such as, TAPPI T205 is required. 1.3 This test method requires specimens such as those described in 1.2. 1.4 While testing is possible on finished paper or paperboard, information on fiber quality from intermediate steps in the pulping or papermaking process, or both, is frequently more useful for improving finished paper and paperboard quality or improving fiber utilization of recycled fibers, or fibers subjected to new pulping, bleaching, or finishing processes (1, 2, 3, 4). 1.5 The modifications of this test method required for testing finished paper is straightforward; however, testing shall be done in the two principle directions of the sheet, as required in Test Method D829. The finished paper or paperboard will generally have nonrandom fiber orientation, resulting in different strength properties in the two principle directions of the finished sheet. Testing of sheets having a grammage greater than 100 g/m , which includes some paper materials described as paper and many paperboards, is difficult because of problems associated with clamping of individual fibers as the number of fibers per unit area increases. 1.6 Modifications such as those in 1.5 are not described in this test method. If modifications are made, they must be acknowledged and clearly described in the report as deviations from the standard procedure. 1.7 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||
2. Referenced Documents | ||||||||||||||
|
Chcete pravidelně odebírat informace o nově vycházejících normách z celého světa a to zcela zdarma?
Přihlašte se k odběru. Vše je velice jednoduché a absolutně ZDARMA.
Na výběr máte vydavatele z celého světa.
Poslední aktualizace: 12.11.2024 (Počet položek: 2 210 658)
© Copyright 2024 NORMSERVIS s.r.o.