Potřebujeme váš souhlas k využití jednotlivých dat, aby se vám mimo jiné mohly ukazovat informace týkající se vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.
Standard Practice for Accelerated Weathering Test Conditions and Procedures for Bituminous Materials (Xenon-Arc Method)
Automaticky přeložený název:
Standardní praxe pro Urychlené stárnutí Zkušební podmínky a postupy pro živičných nerostů (metoda Xenon - Arc )
NORMA vydána dne 1.2.2008
Označení normy: ASTM D4798-08
Poznámka: NEPLATNÁ
Datum vydání normy: 1.2.2008
Kód zboží: NS-28610
Počet stran: 3
Přibližná hmotnost: 9 g (0.02 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
accelerated weathering, bituminous materials, degradation, exposure, light exposure, roofing, ultraviolet, waterproofing, xenon-arc, Accelerated aging/testing--building materials, Bituminous roofing materials, Light exposure, Spray applications/testing, Water spray method, Xenon-arc light exposure, ICS Number Code 75.140 (Waxes, bituminous materials and other petroleum products), 91.100.50 (Binders. Sealing materials), 93.080.20 (Road construction materials)
Significance and Use | ||||||||||||||||
It is not possible to establish a precise correlation between accelerated and natural weathering because (1) there are geographical climatic variations, local weather variations, and variations in local pollutants, and (2) the relation between accelerated and natural weathering is material dependent with differences in acceleration factors between materials as well as for different formulations of the same material. This weathering apparatus and procedure are used for comparing the weathering characteristics of bituminous materials against a control material for which the outdoor weathering characteristics are known. Guide G 141 provides guidance regarding this issue. Note 1—This practice can be used for other than bituminous materials, but the significance and use have not been evaluated. |
||||||||||||||||
1. Scope | ||||||||||||||||
1.1 This practice covers test conditions and procedures for xenon-arc exposures according to Practices G 151 and G 155 for bituminous roofing and waterproofing materials that have a minimum softening point of approximately 95°C (200°F) as determined by Test Method D 36. (Also see Terminology G 113.) 1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||
2. Referenced Documents | ||||||||||||||||
|
Chcete mít jistotu o platnosti užívaných předpisů?
Nabízíme Vám řešení, abyste mohli používat stále platné (aktuální) legislativní předpisy.