Standard Test Method for Simultaneous Thickness and Electrode Potential Determination of Individual Layers in Multilayer Nickel Deposit (STEP Test)
Automaticky přeložený název:
Standardní zkušební metoda pro současné tloušťky a potenciál elektrody Stanovení jednotlivých vrstev ve vícevrstvé Nikl vkladu (STEP Test)
NORMA vydána dne 1.5.2014
Označení normy: ASTM B764-04(2014)
Poznámka: NEPLATNÁ
Datum vydání normy: 1.5.2014
Kód zboží: NS-8017
Počet stran: 6
Přibližná hmotnost: 18 g (0.04 liber)
Země: Americká technická norma
Kategorie: Technické normy ASTM
Keywords:
potential, STEP, thickness, ICS Number Code 25.220.40 (Metallic coatings)
Significance and Use | ||||||
4.1 The ability of a multilayer nickel deposit to enhance corrosion resistance is a function of the difference in the electrode potentials of the nickel layers (as measured individually at a fixed current density in a given electrolyte versus a reference electrode) and the thicknesses of the layers. The potential differences must be sufficient to cause the bright nickel or top layer to corrode preferentially and sacrificially with respect to the semi-bright nickel layer beneath it. 4.2 This test procedure allows the measurement of these potential differences directly on an electroplated part rather than on separate foil specimens in such a way that time determines the thickness of each layer, while the potential difference between nickel layers is an indication of the corrosion resistance of the total nickel deposit. 4.3 The interpretation and evaluation of the results of this test should be by agreement between the purchaser and the manufacturer. 1.1 This test method closely
estimates the thickness of individual layers of a multilayer nickel
electrodeposit and the potential differences between the individual
layers while being anodically stripped at constant current
density.1.2 This test method does not cover
deposit systems other than multilayer electroplated nickel
deposits.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||
2. Referenced Documents | ||||||
|
Historická
1.12.2010
Historická
1.5.2013
Historická
1.1.2014
Historická
1.11.2013
Historická
1.5.2014
Historická
1.11.2011
Chcete mít jistotu, že používáte pouze platné technické normy?
Nabízíme Vám řešení, které Vám zajistí měsíční přehled o aktuálnosti norem, které používáte.
Chcete vědět více informací? Podívejte se na tuto stránku.
Poslední aktualizace: 22.12.2024 (Počet položek: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.