NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
NORMA vydána dne 1.8.1994
Designation standards: SAE AMS5707H
Note: Neaktuální
Publication date standards: 1.8.1994
Country: American technical standard
Kategorie: Technické normy SAE