NORMSERVIS s.r.o.

ASTM A801-09

Standard Specification for Wrought Iron-Cobalt High Magnetic Saturation Alloys (UNS R30005 and K92650)

NORMA vydána dne 1.11.2009

Anglicky -
Online zabezpečené PDF (1791.40 CZK)

Anglicky -
Tištěné (1791.40 CZK)

The information about the standard:

Designation standards: ASTM A801-09
Note: NEPLATNÁ
Publication date standards: 1.11.2009
The number of pages: 5
Approximate weight : 15 g (0.03 lbs)
Country: American technical standard
Kategorie: Technické normy ASTM

Annotation of standard text ASTM A801-09 :

Keywords:
core loss, iron-cobalt alloy, magnetic flux density, magnetic saturation, Electrical conductors, Iron cobalt alloys, Magnetic materials/applications--specifications, Permeability--magnetic alloys, UNS K92650 (Fe-Co soft magnetic alloy), UNS R30005 (Co-Ni-Cr-Mo alloy, MP-35-N), Wrought iron-cobalt alloys, ICS Number Code 77.080.10 (Irons)