ASTM A385/A385M-17 - 1.9.2017
 
1. Scope

1.1 This practice covers the precautions that should be taken to obtain high-quality hot-dip galvanized coatings.

1.2 Where experience on a specific product indicates a relaxing of any provision, the mutually acceptable change shall be a matter for agreement between the manufacturer and purchaser.

1.3 This specification is applicable to orders in either inch-pound units (as A385) or in SI units (as A385M). Inch-pound units and SI units are not necessarily exact equivalents. Within the text of this specification and where appropriate, SI units are shown in brackets. Each system shall be used independently of the other without combining values in any way.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

 
2. Referenced Documents

A123/A123M-17

Standard Specification for Zinc (Hot-Dip Galvanized) Coatings on Iron and Steel Products

A384/A384M-07(2019)

Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies

A153/A153M-23

Standard Specification for Zinc Coating (Hot-Dip) on Iron and Steel Hardware

A143/A143M-07(2020)

Standard Practice for Safeguarding Against Embrittlement of Hot-Dip Galvanized Structural Steel Products and Procedure for Detecting Embrittlement

A563-15

Standard Specification for Carbon and Alloy Steel Nuts